Muna farin cikin amsa kowace tambaya, da fatan za a aiko da tambayoyinku da odar ku.
Aikin | Siga | Naúrar |
Kebul model | OPGW-2S 2×24B1(0/92.6-60)
|
|
Lambar fiber optic | 48 | B1 |
Diamita na waya | 13.2 | mm |
Nauyin igiya | 560± 5 | Kg/km |
Tsarin tsarin tsakiya | 1 × Φ2.6/30AS | mm |
fiber na gani naúrar | 2 × Φ2.5/24B1 | mm |
Tsarin tsarin ciki | 4 × Φ2.5/30AS | mm |
Tsarin tsari na waje | 11 × Φ2.8/30AS | mm |
Ƙididdigar yanki na yanki | 92.6 | mm2 |
Ƙarfin karya mara ƙima | 75 | KN |
juriya na DC | 0.6 | Ω/km |
Gajeren iya aiki na yanzu | 60 | THE2S |
Modulus na elasticity | 132 | G Pa |
Ƙididdigar faɗaɗa na layi | 13.8 | ×10-8/ ℃ |
Matsala zuwa rabo mai nauyi | 14.4 | km |
Hanya mafi kusa | Dama |
|
Tsayayyen radius na curvature | 20D | mm |
Rediyon lanƙwasa mai ƙarfi | 30D | mm |
Yanayin ajiya | -60-85 | ℃ |
Yanayin shigarwa | -40-70 | ℃ |
Yanayin aiki | -60-70 | ℃ |
Nau'in fiber optic | G.652D | |
Attenuation coefficient | @1310nm | ≤0.36 dB/km |
@1383nm | ≤0.35 dB/km | |
@1550nm | ≤0.22dB/km | |
@1625nm | ≤0.23 dB/km | |
Ingantacciyar ƙungiyar refractive index | @1310nm | 1.467 |
@1550nm | 1.467 | |
Watsewar yanayin polarization | ≤0.1ps/√km | |
MFD 1310 nm | 9.0± 0.3um | |
MFD 1550 nm | 10.0± 0.3um | |
Diamita na layin layi | 125.0± 1.0um | |
Rashin da'ira na sutura | ≤1.0% | |
Kuskuren ma'auni / cladding concentricity | ≤0.8 ku | |
Diamita na layin layi | 242±7 ku | |
Core rashin da'ira | ≤6.0% | |
≤12.0am | ||
Kuskuren daidaitawar layin layi/rubutu | ≤1260 nm | |
yankan na USB | 1312± 10 nm | |
Tsayin Watsawa Sifili | 0.092ps/(nm2∙km) | |
gangarawar watsawa | ≤0.05ps/√km |
Mr Herry
Waya/Wechat/Whatsapp:+8618123897029
Skype:sales09@aixton.com
Mr James
Waya/Wechat/Whatsapp:+8618566291592
Skype: aixton05